42CrMoS4 is a direct hardening steel like 42CrMo4 but with controlled sulphur content for improved machinability. The material is stocked in cold drawn hardened and tempered condition.
42CrMoS4Supply Form & Size & Tolerance
Form of Supply
Size(mm)
Length(mm)
Round bar
Φ6-Φ1,000
3,000-10,000
Square bar
100×100-600×600
3,000-6,000
Plate/Sheet
Thickness :20-400
Width:80-1,000
2,000-6,000
Flat bar/Blcoks
Thickness :120-800
Width:120-1,500
2,000-6,000
42CrMoS4Surface Finish&Tolerance
Surface Finish
Black-Forged
Black-Rolled
Turned
Grinding
Polished
Peeled
Cold Drawn
Tolerance
(0,+5mm)
(0,+1mm)
(0,+3mm)
Best h9
Best h11
Best H11
Best H11
42CrMoS4Chemical Composition
Grade
C
Si
Mn
Cr
Mo
P
S
42CrMoS4/1.7227
0.38-0.45
≤ 0.4
0.6-0.9
0.9-1.2
0.15-0.3
≤ 0.025
0.02-0.04
42CrMoS4Relevant Standards
EU
EN
USA
–
Germany
DIN,WNr
France
AFNOR
Italy
UNI
Spain
UNE
Inter
ISO
42CrMoS4
4140
42CrMoS4
42CD4u
42CrMo4
40CrMo41
42CrMoS4
42CrMoS4Mechanical Property
Nominal diameter (mm):
to 16
16 – 40
40 – 100
100 – 160
160 – 250
Rm – Tensile strength (MPa) (+QT)
1100-1300
1000-1200
900-1100
800-950
750-900
Rm – Tensile strength (MPa) (+AC)
630
Nominal diameter(mm): or for flat products thickness: to 8; 8-20; 20-60; 60-100; 100-160;
to 16
16 – 40
40 – 100
100 – 160
160 – 250
Re – Upper yield strength or Rp0.2 – 0.2% proof strength (MPa) (+QT)
900
750
650
550
500
Nominal thickness (mm):
to 16
16 – 40
40 – 100
100 – 160
160 – 250
A – Min. elongation Lo = 5,65 √ So (%) (+QT), round products
10
11
12
13
14
Nominal diameter (mm): or for flat products thickness: to 8; 8-20; 20-60; 60-100; 100-160;
to 16
16 – 40
40 – 100
100 – 160
160 – 250
Z – Reduction in cross section on fracture (%) (+QT)
40
45
50
50
55
Z – Reduction in cross section on fracture (%) (+AC)
58
Brinell hardness (HBW): (+S)
255
Brinell hardness (HBW): (+A)
241
Properties of steel 42CrMoS4 (1.7227)
Weldability: Bad weldability due to the high crack danger.
Hardenability: Medium-good hardenability, suitable for hot purposes till a temperature of 500. It can be hardened in oil.
42CrMoS4Forging
42CrMoS4 forging temperature:900 – 1100°C ,cooling as slowly as possible in still air or in sand after forged.
42CrMoS4Heat Treatment
Normalizing: 850 – 880°C,Cooling in air
Soft Annealing:680 – 720°C,Cooling in furnace
Stress relieve:450-650°C,Cooling in air
Hardening:820 – 880°C,oil or water quench
Tempering:540 – 680°C,Cooling in air
42CrMoS4Surface Hardness
Treated to improve shearability (+S):Max 255HB
Soft annealed (+A):Max 241HB
Pre Quenched and tempered:280-320HB
Flame or induction hardening:Min 53HRC
NORMAL HARDENABILITY +H (850°C – hardness HRC – distance mm)
Distance mm
1.5
3
5
7
9
11
13
15
20
25
30
35
40
45
50
HRC Min
53
53
52
51
49
43
40
37
34
32
31
30
30
29
29
HRC Max
61
61
61
60
60
59
59
58
56
53
51
48
47
46
45
42CrMoS4Application
42CrMoS4 has high strength and wear-resistance,widely used in many industries.
Components with high strength and toughness for tools, automotive parts,mechanical engineering, armament components,such as geer wheels,pinions,connecting rods,parts for mechanical engineering.
Statically and dynamically stressed components for vehicles, engines and machines. For parts of larger cross-sections, crankshafts,gears