Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the translatepress-multilingual domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /home1/sohoweld/public_html/waldunsteel/wp-includes/functions.php on line 6114

Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the wordpress-seo domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /home1/sohoweld/public_html/waldunsteel/wp-includes/functions.php on line 6114
21CrMoV5-7 / 1.7709 Aço - EN 10269 | Waldun Steel

21CrMoV5-11_1.8070

21CrMoV5-11 / 1.8070 Aço

Composição Química de acordo com EN 10269

NOTA NÚMERO C Si Mn P S Cr Mo Ni V
21CrMoV5-11 1.8070 0,17-0,25 0,30-0,60 0,30-0,60 ≤ 0,035 ≤ 0,035 1,20-1,50 1h00-1h20 ≤ 0,60 0,25-0,35

21CrMoV5-11 / 1.8070 Aço Descrição

Aço estrutural especial.

21CrMoV5-11 / 1.8070 Aço Formulários

Parafusos e porcas e componentes forjados para motores de haste até temperaturas de trabalho de no máximo 539 graus.

21CrMoV5-11 / 1.8070 Aço Propriedades mecânicas

Temperatura de trabalho a quente / ℃: 1100 ~ 850
Temperatura de tratamento térmico / ℃ | recozimento / normalização: 650 ~ 740
Temperatura de tratamento térmico / ℃ | têmpera: 900 ~ 950 Óleo ou Ar
Temperatura de tratamento térmico / ℃ | têmpera: 680 ~ 740
HBW: 205 ~ 250
(≥) | σb / MPa: 690 ~ 830
(≥) | σs / MPa: 540
(≥) | δ5 (%): 16
(≥) | AKV / J: 55

MPropriedade mecânica sob alta temperatura

Força de rendimento σ0,2≥ / MPa | 200 ℃: 510
Força de rendimento σ0,2≥ / MPa | 300 ℃: 481
Força de rendimento σ0,2≥ / MPa | 350 ℃: 461
Força de escoamento σ0,2≥ / MPa | 400 ℃: 431
Força de rendimento σ0,2≥ / MPa | 450 ℃: 402
Força de rendimento σ0,2≥ / MPa | 500 ℃: 373

21CrMoV5-11 / 1.8070 Aço UMAFormas Disponíveis  

Barra preta / Barra plana / Barra quadrada / Tubo, / Tira de aço, / Folha

Brilhante - descascado + polimento, desbaste sem centro

Forjado - anel, tubo, revestimento do tubo, discos, eixo

Propriedades físicas (valores médios) à temperatura ambiente

Módulo de elasticidade [103 x N / mm2]: 210 Densidade [g / cm3]: 7,80 Transformação por Resfriamento Contínuo (CCT)

21CrMoV5-11 / 1.8070 Aço Recozimento Suave

Aqueça a 650-740 graus, resfrie lentamente.

21CrMoV5-11 / 1.8070 Aço Endurecimento

Endureça a partir de uma temperatura de 900-950 graus seguida de resfriamento a óleo ou ar.

21CrMoV5-11 / 1.8070 Aço Temperamento

Temperatura de têmpera: 680-740 graus.

21CrMoV5-11 / 1.8070 Aço Forging

Temperatura de formação a quente: 1100-850 graus.