Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the translatepress-multilingual domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /home1/sohoweld/public_html/waldunsteel/wp-includes/functions.php on line 6114

Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the wordpress-seo domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /home1/sohoweld/public_html/waldunsteel/wp-includes/functions.php on line 6114

Notice: La función _load_textdomain_just_in_time ha sido llamada de forma incorrecta. La carga de la traducción para el dominio avia_framework se activó demasiado pronto. Esto suele ser un indicador de que algún código del plugin o tema se ejecuta demasiado pronto. Las traducciones deberían cargarse en la acción init o más tarde. Por favor, ve depuración en WordPress para más información. (Este mensaje fue añadido en la versión 6.7.0). in /home1/sohoweld/public_html/waldunsteel/wp-includes/functions.php on line 6114
18CrNiMo7-6 / 1.6587 Acero - Acero Waldun

18crnimo7 6 225x300

18CrNiMo7-6 / 1.6587 Acero

18CrNiMo7-6 / 1.6587 Acero aleado fabricantes y proveedores, suministrados con varillas redondas, cuadradas / planas, rodillos, ejes, bloques y piezas de forja.

El acero de aleación 18CrNiMo7-6 / 1.6587 es un acero de baja aleación que se puede tratar térmicamente y que contiene níquel, cromo y molibdeno según la norma DIN de Alemania, que es conocido por su tenacidad y capacidad para desarrollar una alta resistencia en la condición de tratamiento térmico al tiempo que conserva una buena resistencia a la fatiga. El acero de aleación 18CrNiMo7-6 / 1.6587 se usa ampliamente en ejes, engranajes, ejes, husillos, acoplamientos, pasadores, etc. de servicio pesado.

Composición química según EN 10084 (acero cementado)

CALIFICACIÓN NÚMERO C Si Minnesota PAG S Cr Mes Ni
18CrNiMo7-6 1.6587 0,15-0,21 ≤ 0,40 0,50-0,90 ≤ 0.025 ≤ 0.035 1,50-1,80 0,25-0,35 1,40-1,70

Tamaño y tolerancia y proceso

Forma Tamaño (mm) Proceso Tolerancia Longitud (mm)
Redondo Φ6-Φ50 Estirado en frío H11 3000-5800
Redondo Φ40-Φ300 Laminado en caliente -0 / + 3 mm 3000-10000
Redondo Φ120-Φ1000 Forjado en caliente -0 / + 3 mm 3000-10000
Plano / Cuadrado / Bloque Espesor: 120-800
Ancho: 120-1500
Forjado en caliente -0 / + 3 mm 500-6000

Tratamiento térmico

Normalizando para 18CrNiMo7-6/1.6587
1.Temperatura de normalización nominal: 840-890 ° C
2.Mantener la temperatura durante varias horas.
3.Enfriamiento en el aire

Recocido Para 18CrNiMo7-6/1.6587
1.Temperatura de recocido nominal: 630-650 ° C
2.Enfríe lentamente en la furia
3.Dureza Brinell máxima de 229

Endurecimiento y revenido (QT) para 18CrNiMo7-6/1.6587
1.Temperatura de endurecimiento nominal: 830-865 ° C
2.Mantener a esta temperatura y luego enfriar en aceite.
3.Temperar lo antes posible cuando la temperatura baja a la temperatura ambiente
4.Calentar el acero con cuidado a una temperatura adecuada seleccionada por referencia a una tabla o tabla de templado
5.La temperatura de revenido habitual es de 600 ° C, que depende de los requisitos reales
6.Mantenga el material fuera del horno, luego enfríe en el aire.

Propiedad mecánica (solo como referencia)

1.Resistencia a la tracción: 980-1270MPa
2.Punto de rendimiento: 780MPa
3.Reducción porcentual del área después de la fractura: 40%
4.Elongación después de la fractura: 11%
5.Prueba de impacto (+ 20 ° C): Longitud - 45 ~ 50J

Condición de entrega

1.Forma: Redondo / Cuadrado / Plano / Ejes / Rodillos / Bloques
2.condición de la superficie: superficie negra / superficie brillante
3.Tratamiento térmico: normalizado / recocido / QT
4.Rectitud: Max 3 mm / m (la rectitud mejorada puede estar disponible a pedido)
5.Longitud: 3000-5800mm adecuado para contenedores de 20 ″. por encima de 6000 mm, adecuado para contenedores de 40 ″
6.Tamaño del grano: 5-8 según ASTM E112-96
7.Dureza típica: HRC28-32
8.Estándar ultrasónico: Sep1921 / ASTM A388 / EN 10228-3
9.Inclusión no metálica: 2 máx. Según ASTM E45 / K4≤20 según DIN 50602
10.Relación de forja: mínimo 4: 1
11.Marcado: Grado / Peso / Longitud / Tamaño / Número de calor

Certificacion de calidad

Se proporcionará un informe de prueba del material (Certificado de inspección EN 10084), que documente lo siguiente:
1.Análisis químico
2.Propiedades mecánicas
3.dureza de la superficie
Inclusión no metálica
5.Proceso de tratamiento térmico
6.tamaño de grano
7.relación de forja
8.Método / criterios de prueba NDE

últimos productos

CONTACTO ACERO WALDUN

Móvil:

+8618652469606

Correo electrónico:

iguhongtao@gmail.com

logotipo de acero waldun iso 9001 300x158

¡Obtenga una cotización ahora!

© Copyright - ACERO WALDUN